Cavitation erosion of WC-Co

Bibliography: pages 68-70.

Saved in:
Bibliographic Details
Main Author: Hankey, S E
Other Authors: Ball, Anthony
Format: Thesis
Language:English
Published: Centre for Materials Engineering 2016
Subjects:
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1867613171904151552
access_status_str Open Access
author Hankey, S E
author2 Ball, Anthony
author_browse Ball, Anthony
Hankey, S E
author_facet Ball, Anthony
Hankey, S E
author_sort Hankey, S E
collection Thesis
description Bibliography: pages 68-70.
format Thesis
id oai:open.uct.ac.za:11427/21135
institution University of Cape Town (South Africa)
language eng
last_indexed 2026-06-10T12:31:54.917Z
license_str Not specified — see source repository
provenance_str_mv Harvested via OAI-PMH from UCTD — University of Cape Town Open Access Repository
publishDate 2016
publishDateRange 2016
publishDateSort 2016
publisher Centre for Materials Engineering
publisherStr Centre for Materials Engineering
record_format dspace
source_str UCTD — University of Cape Town Open Access Repository
spelling oai:open.uct.ac.za:11427/21135 Cavitation erosion of WC-Co Hankey, S E Ball, Anthony Cavitation Tungsten-cobalt alloys - Metallurgy Materials Science Bibliography: pages 68-70. An investigation involving the vibratory cavitation erosion of WC-Co alloys was undertaken in order to determine the mechanisms of material removal. Nineteen grades of WC-Co alloys were studied. These alloys had been previously characterised according to microstructural and mechanical properties. Further characterisation by way of Young's modulus and density of the materials was undertaken. An investigation of the i nfluence of various parameters on cavitation erosion established a binder content dependence on erosion. For two grain sizes, erosion was found to increase to a maximum at 12 vo1-% binder content (1.8 μm grain size) and 23 vol-% binder (2.8 μm grain size). The main mode of material removal was found to be cobalt removal followed by WC grain pull-out. In high binder content alloys, cobalt removal was predominant with little loss of WC grains. X-ray diffraction showed that the allotropic phase transformation of the binder under cavitational attack was beneficial to the erosion resistance of these alloys. The erosion of low binder content alloys was controlled by the contiguity of the WC skeleton. Maximum erosion occurred at binder contents which corresponded to the combination of a fragile WC skeleton and a small volume of available cobalt for strain induced transformation. 2016-08-05T10:49:21Z 2016-08-05T10:49:21Z 1987 Master Thesis Masters MSc http://hdl.handle.net/11427/21135 eng application/pdf Centre for Materials Engineering Faculty of Engineering and the Built Environment University of Cape Town
spellingShingle Cavitation
Tungsten-cobalt alloys - Metallurgy
Materials Science
Hankey, S E
Cavitation erosion of WC-Co
thesis_degree_str Master's
title Cavitation erosion of WC-Co
title_full Cavitation erosion of WC-Co
title_fullStr Cavitation erosion of WC-Co
title_full_unstemmed Cavitation erosion of WC-Co
title_short Cavitation erosion of WC-Co
title_sort cavitation erosion of wc co
topic Cavitation
Tungsten-cobalt alloys - Metallurgy
Materials Science
url http://hdl.handle.net/11427/21135
work_keys_str_mv AT hankeyse cavitationerosionofwcco